THE technically advanced PRE-DOSED NON GAMMA 2 fine grain 48% Amalgam Powder, with high strength ensures longevity and patient satisfaction. The alloy to mercury ratio 1:1 ready for mixing on a amalgamator. The compressive strength of PYRAX ALOYSIL at 24 hours is 510 MPa, and the dimensional change during hardening is +0.02%.
COMPOSITION:
Ag 48% Sn 23.3% Cu 28.7%